- 拉伸強度 [MPa]: 4.07
- 脆化溫度 [℃]: -56.0
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
| Hardness, Shore A | 55 | 55 | Instant; ASTM D2240 |
| Tensile Strength, Yield | 4.07 MPa | 590 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
| 2.45 MPa @Strain 300 % | 355 psi @Strain 300 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 | |
| Elongation at Break | 580 % | 580 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
| Rebound | 43 % | 43 % | Bayshore; ASTM D2632 |
| Tear Strength | 22.1 kN/m | 126 pli | Die C (graves), 20 in/min; ASTM D624 |
| Compression Set | 13 % | 13 % | Method B, 73°F(23°C), 22 hrs; ASTM D395 |
| Thermal Properties | Metric | English | Comments |
| Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
| Flammability, UL94 | V-0 | V-0 | Natural, 0.062 in thick; UL 94 |
| Oxygen Index | 27 % | 27 % | Limiting, 0.062 in bars; ASTM D2863 |