| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Specific Gravity | 1.30 g/cc @Temperature 23.0 °C | 1.30 g/cc @Temperature 73.4 °F | ISO 1183 | ||
| Moisture Absorption at Equilibrium | 0.040 % @Temperature 23.0 °C, Time 86400 sec | 0.040 % @Temperature 73.4 °F, Time 24.0 hour | 50% RH; ISO 62 | ||
| Mechanical Properties | Metric | English | Comments | ||
| Tensile Strength at Break | 120 MPa @Temperature 23.0 °C | 17400 psi @Temperature 73.4 °F | ISO 527 | ||
| Elongation at Break | >= 150 % @Temperature 23.0 °C | >= 150 % @Temperature 73.4 °F | ISO 527 | ||
| Tensile Modulus | 2.80 GPa @Temperature 23.0 °C | 406 ksi @Temperature 73.4 °F | ISO 527 | ||
| Tear Strength | 6.70 kN/m @Temperature 23.0 °C | 38.2 pli @Temperature 73.4 °F | |||
| Electrical Properties | Metric | English | Comments | ||
| Volume Resistivity | 4.00e+16 ohm-cm @Temperature 23.0 °C | 4.00e+16 ohm-cm @Temperature 73.4 °F | 100V; ASTM D257 | ||
| Dielectric Constant | 3.5 @Frequency 1e+7 Hz, Temperature 23.0 °C | 3.5 @Frequency 1e+7 Hz, Temperature 73.4 °F | |||
| Dielectric Strength | 190 kV/mm @Temperature 23.0 °C | 4830 kV/in @Temperature 73.4 °F | 1/4 inch electrode; ASTM D149 | ||
| Dissipation Factor | 0.0020 @Frequency 1e+7 Hz, Temperature 23.0 °C | 0.0020 @Frequency 1e+7 Hz, Temperature 73.4 °F | ASTM D150 | ||
| Thermal Properties | Metric | English | Comments | ||
| CTE, linear | 47.0 μm/m-°C | 26.1 μin/in-°F | MD, below Tg; ASTM D696 | ||
| Shrinkage | >= 2.0 % @Temperature 200 °C | >= 2.0 % @Temperature 392 °F | TM-VX-84 | ||
| Descriptive Properties | |||||
| Puncture Strength (kJ/m2) | 26 | Def Stan 81-75; 23°C | |||