填料/增強材料: 礦物填料
特性: 電鍍
加工方法: 注射成型
多點數據: Elastic Modulus vs Temperature (ASTM D4065),Flexural DMA (ASTM D4065),Instrumented Impact (Energy) (ASTM D3763),Instrumented Impact (Load) (ASTM D3763),Pressure-Volume-Temperature (PVT - Zoller Method),Shear DMA (ASTM D4065),Specific Heat vs. Temperature (ASTM D3417),Tensile Creep (ASTM D2990),Tensile Fatigue,Tensile Stress vs. Strain (ASTM D638),Thermal Conductivity vs. Temperature (ASTM E1530),Viscosity vs. Shear Rate (ASTM D3835)
- 模具溫度 °C
- 背壓 MPa
- 射嘴溫度 °C
- 建議的最大水分含量 0.020 %
- 加工(熔體)溫度 °C
- 無缺口懸臂梁沖擊 390 J/m ASTM D4812
- 干燥溫度 121 °C
- 建議的最大水分含量 0.020 %
- 背壓 MPa
- 載荷下熱變形溫度 ASTM D648