特性: 耐低溫沖擊,耐化學性良好
加工方法: 注射成型
多點數據: Coefficient of Thermal Expansion vs. Temperature (ASTM E831),Compressive Stress vs. Strain (ASTM D695),Flexural DMA (ASTM D4065),Instrumented Impact (Energy) (ASTM D3763),Instrumented Impact (Load) (ASTM D3763),Shear DMA (ASTM D4065),Specific Heat vs. Temperature (ASTM D3417),Tensile Creep (ASTM D2990),Tensile Stress vs. Strain (ASTM D638),Thermal Conductivity vs. Temperature (ASTM E1530),Viscosity vs. Shear Rate (ASTM D3835)
- 懸壁梁缺口沖擊強度 ASTM D256
- 收縮率 - 流動 % 內部方法
- 建議的最大水分含量 0.020 %
- 無缺口懸臂梁沖擊 3200 J/m ASTM D4812
- 彎曲強度 68.9 MPa ASTM D790
- 干燥溫度 110 °C
- 伸長率 170 % ASTM D638
- 螺桿轉速 rpm
- 載荷下熱變形溫度 ASTM D648
- 加工(熔體)溫度 °C