| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 | ||
| Viscosity | 111000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
111000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 | ||
| 129000 cP @Shear Rate 5000 1/s, Temperature 215 °C |
129000 cP @Shear Rate 5000 1/s, Temperature 419 °F |
ISO 11403-1 -2 | |||
| 152000 cP @Shear Rate 5000 1/s, Temperature 200 °C |
152000 cP @Shear Rate 5000 1/s, Temperature 392 °F |
ISO 11403-1 -2 | |||
| 432000 cP @Shear Rate 500 1/s, Temperature 230 °C |
432000 cP @Shear Rate 500 1/s, Temperature 446 °F |
ISO 11403-1 -2 | |||
| 502000 cP @Shear Rate 500 1/s, Temperature 215 °C |
502000 cP @Shear Rate 500 1/s, Temperature 419 °F |
ISO 11403-1 -2 | |||
| 593000 cP @Shear Rate 500 1/s, Temperature 200 °C |
593000 cP @Shear Rate 500 1/s, Temperature 392 °F |
ISO 11403-1 -2 | |||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 2577 | ||
| Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 | ||
| Melt Flow | 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 | ||
| Mechanical Properties | Metric | English | Comments | ||
| Tensile Stress | 44.9 MPa @Strain 2.20 %, Temperature 23.0 °C |
6510 psi @Strain 2.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 | ||
| 57.6 MPa @Strain 1.80 %, Temperature -40.0 °C |
8350 psi @Strain 1.80 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |||
| 64.5 MPa @Strain 8.00 %, Temperature 23.0 °C |
9350 psi @Strain 8.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |||
| 65.6 MPa @Strain 15.0 %, Temperature 23.0 °C |
9510 psi @Strain 15.0 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |||
| 94.1 MPa @Strain 7.00 %, Temperature -40.0 °C |
13600 psi @Strain 7.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |||
| 96.0 MPa @Strain 13.0 %, Temperature -40.0 °C |
13900 psi @Strain 13.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |||
| Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 | ||
| Elongation at Break | 45 % | 45 % | Nominal; ISO 527-1/-2 | ||
| Elongation at Yield | 18 % | 18 % | ISO 527-1/-2 | ||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 | ||
| Flexural Modulus | 2.80 GPa | 406 ksi | ISO 178 | ||
| Secant Modulus | 0.140526 GPa @Strain 19.0 %, Temperature 100 °C |
20.3819 ksi @Strain 19.0 %, Temperature 212 °F |
ISO 11403-1 -2 | ||
| 0.191579 GPa @Strain 19.0 %, Temperature 80.0 °C |
27.7866 ksi @Strain 19.0 %, Temperature 176 °F |
ISO 11403-1 -2 | |||
| 0.285556 GPa @Strain 9.00 %, Temperature 100 °C |
41.4170 ksi @Strain 9.00 %, Temperature 212 °F |
ISO 11403-1 -2 | |||
| 0.386471 GPa @Strain 17.0 %, Temperature 23.0 °C |
56.0538 ksi @Strain 17.0 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |||
| 0.393333 GPa @Strain 9.00 %, Temperature 80.0 °C |
57.0490 ksi @Strain 9.00 %, Temperature 176 °F |
ISO 11403-1 -2 | |||
| 0.640 GPa @Strain 15.0 %, Temperature -40.0 °C |
92.8 ksi @Strain 15.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |||
| 0.80625 GPa @Strain 8.00 %, Temperature 23.0 °C |
116.94 ksi @Strain 8.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |||
| 0.854167 GPa @Strain 2.40 %, Temperature 100 °C |
123.888 ksi @Strain 2.40 %, Temperature 212 °F |
ISO 11403-1 -2 | |||
| 1.14167 GPa @Strain 2.40 %, Temperature 80.0 °C |
165.588 ksi @Strain 2.40 %, Temperature 176 °F |
ISO 11403-1 -2 | |||
| 1.34429 GPa @Strain 7.00 %, Temperature -40.0 °C |
194.976 ksi @Strain 7.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |||
| 2.04091 GPa @Strain 2.20 %, Temperature 23.0 °C |
296.014 ksi @Strain 2.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |||
| 3.20 GPa @Strain 1.80 %, Temperature -40.0 °C |
464 ksi @Strain 1.80 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ISO 180/1A | ||
| Charpy Impact Unnotched | 25.0 J/cm² | 119 ft-lb/in² | ISO 179/1eU | ||
| 17.0 J/cm² @Temperature -30.0 °C |
80.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179/1eA | ||
| 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA | |||
| Thermal Properties | Metric | English | Comments | ||
| CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 | ||
| CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 | ||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 | ||
| Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 | ||
| Deflection Temperature at 1.8 MPa (264 psi) | 97.0 °C | 207 °F | ISO 75-1/-2 | ||
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
IEC 60695-11-10 | ||
| HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
IEC 60695-11-10 | |||
| De |
|||||
| Additives | Lubricants | ||||
| Release agent | |||||
| Delivery form | Pellets | ||||
| Emissions | <8 mg/kg | VDA 275 | |||
| Part Marking Code | >POM-S< | ISO 11469 | |||
| Processing | Injection Moulding | ||||
| Other Extrusion | |||||
| Profile Extrusion | |||||
| Sheet Extrusion | |||||
| Regional Availability | Asia Pacific | ||||
| Europe | |||||
| Global | |||||
| Near East/Africa | |||||
| North America | |||||
| South and Central America | |||||
| Resin Identification | POM-S | ISO 1043 | |||
| UL recognition | UL | ||||
| UL | |||||
POM 的簡介
POM強(qiáng)度、剛度高,彈性好,減磨耐磨性好。其力學(xué)性能優(yōu)異,比強(qiáng)度可達(dá)50.5MPa,比剛度可達(dá)2650MPa,與金屬十分接近。POM的力學(xué)性能隨溫度變化小,共聚POM比均聚POM的變化稍大一點(diǎn)。
POM的沖擊強(qiáng)度較高,但常規(guī)沖擊不及ABS和PC;POM對缺口敏感,有缺口可使沖擊強(qiáng)度下降90%之多。
POM的疲勞強(qiáng)度十分突出,10交變載荷作用后,疲勞強(qiáng)度可達(dá)35MPa,而PA和PC僅為28MPa。
POM的蠕變性與PA相似,在20℃、21MPa、3000h時(shí)僅為2.3%,而且受溫度的影響很小。
POM的摩擦因數(shù)小,耐磨性好(POM>PA66>PA6>ABS>HPVC>PS>PC),極限PV值很大,自潤滑性好。
POM制品對磨時(shí),高載荷作用時(shí)易產(chǎn)生類似尖叫的噪聲。
POM 化學(xué)性質(zhì)
POM 按分子鏈結(jié)構(gòu)不同,聚甲醛可分為均聚甲醛和共聚甲醛,前者密度、結(jié)晶度、熔點(diǎn)都高,但是熱穩(wěn)定性差,加工溫度窄(10度),對酸堿的穩(wěn)定性略低;后者密度、結(jié)晶度、熔點(diǎn)較低,但熱穩(wěn)定性好,不易分解,加工溫度寬(50度) 。
POM 不足之處在于:由受強(qiáng)酸腐蝕,耐侯差,粘合性差,熱分解與軟化溫度接近,限氧指數(shù)小。它們廣泛用于汽車工業(yè),電子電器,機(jī)械設(shè)備等。還可以做水龍頭、框窗、洗漱盆。
POM具有很低的摩擦系數(shù)和很好的幾何穩(wěn)定性,特別適合于制作齒輪和軸承。由于它還具有耐高溫特性,因此還用于管道器件(管道閥門、泵殼體),草坪設(shè)備等。
POM 環(huán)境性能:
POM不耐強(qiáng)酸和氧化劑,對烯酸及弱酸有一定的穩(wěn)定性。
POM的耐溶劑性良好,可耐烴類、醇類、醛類、醚類、汽油、潤滑油及弱堿等,并可在高溫下保持相當(dāng)?shù)幕瘜W(xué)穩(wěn)定性。吸水性小,尺寸穩(wěn)定性好。
POM的耐候性不好,長期在紫外線作用下,力學(xué)性能下降,表面發(fā)生粉化和龜裂。
應(yīng)用范圍
POM屬結(jié)晶性塑料,熔點(diǎn)明顯,一旦達(dá)到熔點(diǎn),熔體粘度迅速下降。當(dāng)溫度超過一定限度或熔體受熱時(shí)間過長,會(huì)引起分解。
POM具有較好的綜合性能,在熱塑性塑料中是最堅(jiān)硬的,是塑料材料中力學(xué)性能最接近金屬的品種之一,其抗張強(qiáng)度、彎曲強(qiáng)度、耐疲勞強(qiáng)度,耐磨性和電性都十分優(yōu)良,可在-40度--100度之間長期使用。
上海松翰塑化科技有限公司,供應(yīng)原料,品質(zhì)真實(shí),物實(shí)價(jià)廉。
PA6T,46,9T、PC、PC/ABS、PBT、ABS、PPA、PPS、POM、PMMA、TPE、PPO、LCP液晶聚合物。
歡迎各位客戶前來咨詢:
聯(lián)系人: 夏先生
手 機(jī):13501802636
QQ :205730283
郵 箱 :205730283@qq.com
參考圖如下: